Fluropon®
Fluropon® is a premium fluoropolymer coating containing 70% Kynar 500® or Hylar 5000® proprietary resins. Fluropon is a field-proven, high performance exterior quality finish for architectural use. It provides outstanding resistance to ultraviolet radiation resulting in exceptional color retention, resistance to chalking and chemical degradation.
Coating Specifications - Color Change (ASTM D 2244) No more than 5Δ Hunter units at 20 years.
- Chalk Resistance (ASTM D 4214) Rating no less than 8 at 20 years.
- Specular Gloss at 60° (ASTM D 523) Typical: 20-35
- Dew Cycle Weatherometer Test (ASTM D 3361) Passes 1,000 hours. Color change no more than 5Δ Hunter units and chalk rating no less than 8.
- Humidity Resistance (ASTM D 2247) 100% relative humidity. Passes 2,000 hours with no field blisters.
- Salt Spray Resistance (ASTM B 117) Passes 1,000 hours with no blisters and ≤ 1/16" creep from scribe.
- T-Bend (ASTM D 4145) 0T to 3T. No loss of adhesion.
- Impact Resistance Test, Reverse Impact (ASTM D 2794) 3x metal thickness inch-pounds. No loss of adhesion.
- Abrasion Resistance Test, Falling Sand (ASTM D 968) 65 ± 10 liters
- Pencil Hardness (ASTM D 3363) HB to 2H
- Cross Hatch Adhesion (ASTM D 3359) No loss of adhesion
|
|